Yes you can certainly do that. It is quite common and a recommended method to coat with GlassCast 3 as GlassCast 3 self levels to a very smooth surface - much smoother than the other resins, and hence is ideal to do a nice surface layer without the need for any surface finishing.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|