Hi,

I have seen a lot of people building their own ovens.
My question is, with out any knowledge of wiring or programming. Is it hard to connect a temp controller to an oven an get it to work properly ? Or would it be better to buy an oven from Easycomposite ?

Best regards
Replies
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
  


This is my DIY oven built about 14 years ago. 2" thick steel skin insulated panels with polyurethane foam core. 4m long x 1.1m x 1.1m. It runs 100C cooks day after day. Faultless. 
Air is drawn into the two fans and behind the alloy panel, then down and out the open bottom blowing across the finned electric elements.
Paid a control specialist to set up a controller with box and relays for me. Cost about $1000 just for that but I am sure you can buy these types of controllers for about $300.





Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Fasta - 12/31/2018 3:54:28 PM
Click To Enlarge   Click To Enlarge
Click To Enlarge

This is my DIY oven built about 14 years ago. 2" thick steel skin insulated panels with polyurethane foam core. 4m long x 1.1m x 1.1m. It runs 100C cooks day after day. Faultless. 
Air is drawn into the two fans and behind the alloy panel, then down and out the open bottom blowing across the finned electric elements.
Paid a control specialist to set up a controller with box and relays for me. Cost about $1000 just for that but I am sure you can buy these types of controllers for about $300.

Nice.

Hansson43
H
Supreme Being (234 reputation)Supreme Being (234 reputation)Supreme Being (234 reputation)Supreme Being (234 reputation)Supreme Being (234 reputation)Supreme Being (234 reputation)Supreme Being (234 reputation)Supreme Being (234 reputation)Supreme Being (234 reputation)
Group: Forum Members
Posts: 23, Visits: 2.1K
Thanks for the input. Nice build!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search