Using bags for bagging?


Author
Message
ian.g
i
Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)
Group: Forum Members
Posts: 22, Visits: 96
Reading over some forum topics it seems that the sealing of bagging material to flanges causes a lot of problems?
If a piece is small enough then would putting the mould in a bag not be a better solution then there is only one seal to make at the bag mouth - which should be much easier than trying to tape onto a mould which might also not be 100% airtight?
Added advantage is then that you don't need a mould with a flange?

What don't I understand?
Reply
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
ian.g - 12/29/2018 12:19:24 PM
Reading over some forum topics it seems that the sealing of bagging material to flanges causes a lot of problems?
If a piece is small enough then would putting the mould in a bag not be a better solution then there is only one seal to make at the bag mouth - which should be much easier than trying to tape onto a mould which might also not be 100% airtight?
Added advantage is then that you don't need a mould with a flange?

What don't I understand?

I often use bags. Even used a bag for my car's front clip :-)







GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search