Group: Forum Members
Posts: 680,
Visits: 1.9K
|
Hi Rob,
Well, 2 layers of carbon either side fo the Soric will certainly ensure that you don't see any Soric through the gaps in the weave on the first layer of carbon, will certainly block any print from the Soric and it will add considerably more strength to the part so it's worth considering. Whether you need this extra strength would depend on the actual shape of the part and what work it will be doing.
I would strongly suggest making a test laminate up of both of these and infusing in the way that you've planned (a matched tool - so maybe infuse the test panel between 2 sheets of glass) to see how they behave. You can also time the infusion to get a good idea of how long you'll need for the full sized panel.
All the best, Matt