Hi, I plan to make a part that is approx 2m long and 30cm high. I'll be using 2 moulds to create a class A finish on both sides. The stack will consist of 200gsm CF / Soric / Soric / 200gsm CF. I've used 2 layers of soric as i understand one side is smooth to prevent print through of the hex shapes of the soric......or i have i got that wrong? Would i need multiple resin inlet and vac lines to infuse over a 2m distance?