Hi everyone.
I am in the middle of my first carbon project which is linked to here:
http://frankiepix.de/carbon-front-fender-701-supermoto/

The project is blogged in German, but I think that google can translate it very easy.
Though I am German, I would be very happy for every hint I can get.
Regards
Frank

Replies
Frank
Frank
Supreme Being (266 reputation)Supreme Being (266 reputation)Supreme Being (266 reputation)Supreme Being (266 reputation)Supreme Being (266 reputation)Supreme Being (266 reputation)Supreme Being (266 reputation)Supreme Being (266 reputation)Supreme Being (266 reputation)
Group: Forum Members
Posts: 27, Visits: 123
The fourth demoulded component is in order but can be improved.
1. Fault inside

2. Wall thickness in corner

3. Air bubble in the assembly area

4. Pinholes

5. Visibility of the mounting layer

6. Mold release edge clearly visible


It is very difficult for me, to drape the visible layer without wrinkles in the corner.
Perhaps a 45 degree cut can give the reinforcement a better drapability?
regards
Frank
Lester Populaire
L
Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
Frank - 12/12/2018 12:29:34 PM
The fourth demoulded component is in order but can be improved.
1. Fault inside

2. Wall thickness in corner

3. Air bubble in the assembly area

4. Pinholes

5. Visibility of the mounting layer

6. Mold release edge clearly visible


It is very difficult for me, to drape the visible layer without wrinkles in the corner.
Perhaps a 45 degree cut can give the reinforcement a better drapability?
regards
Frank

Looks very good i would say. I think cutting the fabric at 45° would make things worse as it is going ot move around more but you still need to get in the corners just right. I assume you are using a spray tack to hold the fabrics in place? I think it is just a learning process. start in the center and work your way out. make some dabbers to push the fabric into tight corners. Once the fabric is tightly pressed against the mould the pinholes will drastically improve as well.

If it doesn't work out i would cut the fabric along the tight radius and then have another patch overlapping by 10mm or so. as there will be a highlight on the tight radius in most circumstances this is hardly visible.

cheers, Lester

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
oberflaeche - 8 Years Ago
SleepingAwake - 8 Years Ago
Barnsley-Bill - 8 Years Ago
oberflaeche - 8 Years Ago
Hanaldo - 8 Years Ago
oberflaeche - 8 Years Ago
Hanaldo - 8 Years Ago
oberflaeche - 8 Years Ago
oberflaeche - 8 Years Ago
oekmont - 8 Years Ago
oberflaeche - 8 Years Ago
oberflaeche - 8 Years Ago
oberflaeche - 8 Years Ago
SleepingAwake - 8 Years Ago
oberflaeche - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search