By oberflaeche - 11/20/2018 11:21:43 AM				
            
                      
            Hi everyone. I am in the middle of my first carbon project which is linked to here:  http://frankiepix.de/carbon-front-fender-701-supermoto/
  The project is blogged in German, but I think that google can translate it very easy. Though I am German, I would be very happy for every hint I can get. Regards Frank 
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By oberflaeche - 1/9/2019 7:55:47 AM				
            
                      
            For the last front fender, I did not fill the mounting area (picture 3, first page) with chopped carbon fibre thickened resin as usual, but rather with dry carbon fabric. Just as the rest of the mold in the vacuum injection process. With a decent result. The mounting area was completely infused with resin during the infusion and is now just as stable as the rest of the component. Picture will follow... Regards Frank
           
		 | 			
		 
	
	
						
		 	
		
	 |