Hi!
I will CNC cut a plug from Polystyrene foam and will buy the Easycomposites  "Uni-Mould Complete Mould Making Kit "
My question is:
How can I get a smooth surface at the finished foam-plug before I put gelcoat on?
Is there some kind of product that would be suitable for this?


The plug is 1800 mm long and 600 mm wide.

Have a great day!
Regards.
Joel

Edited 8 Years Ago by Joel Illerhag
Fasta
Fasta
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Joel Illerhag - 12/2/2018 10:40:12 PM

Hi!
I will CNC cut a plug from Polystyrene foam and will buy the Easycomposites  "Uni-Mould Complete Mould Making Kit "
My question is:
How can I get a smooth surface at the finished foam-plug before I put gelcoat on?
Is there some kind of product that would be suitable for this?


The plug is 1800 mm long and 600 mm wide.

Have a great day!
Regards.
Joel

Assuming that is a violin for this small size it would be nice to simply use the tooling board materials which can then be sealed.

A foam surface would need at least some light fiberglass and a suitable paint to get your smooth pattern ready for moulding. If you try to paint directly on to a foam it can be difficult to sand as the the foam behind is soft and easily gouged etc when doing this hand sanding. You could also use a suitable timber for CNC machining like Jelutong or even just MDF boards slabbed to be thick enough. 





Joel Illerhag
Joel Illerhag
Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)
Group: Forum Members
Posts: 14, Visits: 37
Hi Fasta!
Thanks for your answer.
It seam to be a good idea to put glassfiber on top of the foam.

I saw a guy that is using "epoxy fairing compound" or putty to flatten out the glassfiber after sanding. I guess I can use that. It might be the same as "Filler" that makes the epoxy thicker with higher viscosity.

It is a double bass by the way :-)

Cheers!
/Joel
Edited 8 Years Ago by Joel Illerhag
Fasta
Fasta
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Ok a bit bigger then.

It just seems that since you have CNC to accurately make a nice pattern that a firmer material will better replicate the CNC. 
With some general strength better than a typical polystyrene. Maybe urethane foams? or even PVC foam$? Then it safer and easier to do hand work on thereafter and without fibreglass even. .

If you were to glass a polystrene foam you could try the really light tissue type fibreglass wet out with epoxy resin, let cure and then the epoxy fairing paste you are thinking of.
There are additives to make your own fairing type paste like Q cells and microballoon powders to add but these are different to the ones that make thicker resin. A thicker resin is like making a glue and these glue additives make a resin that is denser and very hard to sand. The sanding fairing type filler must be used or you can buy epoxy faring pastes as A + B kits ready to go. Resin suppliers like easy composites could have this ? or any marine shop can be a good source for these things.

 




Edited 8 Years Ago by Fasta
Joel Illerhag
Joel Illerhag
Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)
Group: Forum Members
Posts: 14, Visits: 37
Thanks Fasta,
A very good advice about not using dens epoxy. It would be a nightmare to sand down.

I will definatly go for "epoxy faring pastes". I found this at easycomposites: 
https://www.easycomposites.co.uk/emp60-epoxy-moulding-paste

And I will go and see what kind of foams they have in the local shop. PVC or urethane foam sound like a good alternative to the standard white 
polystyrene


Thanks a lot!

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search