Attaching table legs to resin


Author
Message
Bhamoggy
B
Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)
Group: Forum Members
Posts: 38, Visits: 420
What is the best way to attach legs to solid resin?
Can it be drilled and tapped? What’s the best way for something like this?


so we ll go no more a roving meaning
Warren (Staff)
Warren (Staff)
Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
It can be screwed into no problem.  However on a big table like that, you need to be able to hide the fixings as they will show from above otherwise.  You can screw into the wood sections using a structural adhesive for the surface of the leg.  Care will need to be taken to ensure no air is trapped in the bond line otherwise it may be visible from above.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search