Talk Composites - The Forum for Advanced Composites

Attaching table legs to resin

http://www.talkcomposites.com/Topic31011.aspx

By Bhamoggy - 11/16/2018 10:11:30 AM

What is the best way to attach legs to solid resin?
Can it be drilled and tapped? What’s the best way for something like this?


so we ll go no more a roving meaning
By Warren (Staff) - 11/16/2018 12:47:34 PM

It can be screwed into no problem.  However on a big table like that, you need to be able to hide the fixings as they will show from above otherwise.  You can screw into the wood sections using a structural adhesive for the surface of the leg.  Care will need to be taken to ensure no air is trapped in the bond line otherwise it may be visible from above.