I am an old git trying to waterproof a new model boat using EL2 Epoxy Laminating Resin.  The planks are Mahogany and I have stained it with Ronseal mahogany dye, then grain filled it with grain filler.  I have carried out a test using spare wood and the resin looks good when applied but forms streaks and separates after a few minutes.  I have also tried it after applying 25g Woven Glass Ultra Light Plain Weave, this gives it an orange peal effect.  What am I doing wrong.  Help please
Roy. 
Reply
Roy Walton
Roy Walton
Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)
Group: Forum Members
Posts: 5, Visits: 6
Warren (Staff) - 11/15/2018 5:28:17 PM
Sounds like the surface needs a key with sandpaper and a clean as something on the wood surface is causing the resin to be repelled and separating out as you describe.   Certainly like that you are unlikely to get a good bond.

Thanks for the prompt reply.  I will key the surface, clean it and give it a go.
Regards Roy.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Roy Walton - 7 Years Ago
Warren (Staff) - 7 Years Ago
Roy Walton - 7 Years Ago
Roy Walton - 7 Years Ago
Warren (Staff) - 7 Years Ago
Roy Walton - 7 Years Ago
Warren (Staff) - 7 Years Ago
Roy Walton - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search