Group: Forum Members
Posts: 5,
Visits: 6
|
I am an old git trying to waterproof a new model boat using EL2 Epoxy Laminating Resin. The planks are Mahogany and I have stained it with Ronseal mahogany dye, then grain filled it with grain filler. I have carried out a test using spare wood and the resin looks good when applied but forms streaks and separates after a few minutes. I have also tried it after applying 25g Woven Glass Ultra Light Plain Weave, this gives it an orange peal effect. What am I doing wrong. Help please Roy.
|