I'm finding that I can't get rid of the bubbles in the resin cup prior to doing an infusion and I need a degassing chamber.
I've seen them advertised but if I'm correct you put the resin cup in the chamber and pull a negative pressure same as the resin infusion extraction system.... So could I in theory just use the little resin infusion chamber I have now?
If so I might make a slightly larger chamber and put a link to the pump and pull a pressure to it as same time as the part as required?
If this isn't would can someone exactly explain were my understanding is wrong :-)
|