Yeh, mould cant handle it. At that temperature, your mould surface will likely be the first thing to suffer. Depending on the geometry of your part and the layup of your mould, you could definitely experience distortion as well.
Some people dont mind pushing the Tg of their mould, but I'd advise against it. Find out if your pre-preg can do a lower temp initial cure and then post cure it out of the mould, or find a more suitable mould material.
|