Group: Forum Members
Posts: 4,
Visits: 38
|
Hi! I have a Plug that I have sanded to a finish and I was about to make a mold for it using V/E tooling gel coat with a Heat distortion Temperature of 200 Degrees Farenheit. However, I need to bake my prepreg carbon fiber at 250 degrees and I am confused as to whether the tolling gel coat and the vinylester laminating resin with the Chopped Strand Mat will begin to deform at 250 so as to affect the shape of my carbon fiber or impede demolding.
|