I'm in the process of building a CF mountain bike frame , i made three parts (main triangle , chainstay fork ,seatstay fork ). Now i need an adhesive to glue together those parts as strong as possible . Although i plan to wrap some extra cf around the joints afterwards (for extra support) , i need the initial bond to be super strong .What would be my best option ? Any application advice ? I am in Greece so a EU seller with EU shipping would be great .

Reply
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
f1rob - 10/16/2018 11:54:18 AM
If you want the ultimate you could use hysol9394
That beats everything !
Araldite 4858 beats the 3m in peel tests but I would still go with the  3m
Very easy to do your own peel tests and see how the video compares

Thanks Rob. Just need to find where I can buy some :-)