I'm in the process of building a CF mountain bike frame , i made three parts (main triangle , chainstay fork ,seatstay fork ). Now i need an adhesive to glue together those parts as strong as possible . Although i plan to wrap some extra cf around the joints afterwards (for extra support) , i need the initial bond to be super strong .What would be my best option ? Any application advice ? I am in Greece so a EU seller with EU shipping would be great .

Replies
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
9323 is pretty much what most f1 cars are 'glued' together with,on aircraft we use 9396 or similar

But ive bonded bike frames with DP490 and similar cold bonding materials.

The key to the process, is having a nice clean bond area and using a bit of clamping  force to keep it together whilst the bond cures.

Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
scottracing - 10/15/2018 10:17:44 PM
9323 is pretty much what most f1 cars are 'glued' together with,on aircraft we use 9396 or similar

But ive bonded bike frames with DP490 and similar cold bonding materials.

The key to the process, is having a nice clean bond area and using a bit of clamping  force to keep it together whilst the bond cures.

Does 9323 produce a stronger bond than VM100, or is it unnoticeable at my level of construction? 