I'm in the process of building a CF mountain bike frame , i made three parts (main triangle , chainstay fork ,seatstay fork ). Now i need an adhesive to glue together those parts as strong as possible . Although i plan to wrap some extra cf around the joints afterwards (for extra support) , i need the initial bond to be super strong .What would be my best option ? Any application advice ? I am in Greece so a EU seller with EU shipping would be great .

Reply
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
f1rob - 10/15/2018 6:36:23 PM
Myself would use 3m9323  will be perfect for what you want
How does this compare to Easycomposites' VuduGlu VM100?