Hi guys, I’m going to being a resin table soon which will be half wood and half resin, I’m looking to use hairpin legs of which 2 will be into the wood and 2 into the resin. What would be the best way to fix into the resin? I’ve tried searching the web but haven’t really found anything.
Reply
TomH
T
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 4, Visits: 55
Warren (Staff) - 10/16/2018 3:24:12 PM
You can bond to or insert fixings in the resin for the legs, however, if it is in an area of resin, it will be visible on the top of the table so you may need to take that into consideration.

Thanks Warren, I’m looking to use the silver pearl ex for the resin so it will hopefully mean any fixings aren’t visible! 


Is it possible to screw into the resin, tap it to take a bolt or fix a threaded insert into it?
Edited 7 Years Ago by TomH
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search