By TomH - 10/16/2018 1:46:52 PM
Hi guys, I’m going to being a resin table soon which will be half wood and half resin, I’m looking to use hairpin legs of which 2 will be into the wood and 2 into the resin. What would be the best way to fix into the resin? I’ve tried searching the web but haven’t really found anything.
|
By Warren (Staff) - 10/17/2018 8:56:40 AM
You ideally want a fixing that will spread the load a little.
However most good quality hairpin style legs have a large flat plate with 4 or more screw holes to locate, in which case you will likely be fine going into the resin direct.
|
|