Vacuum Bag Kit, No instructions...


Author
Message
surferx
surferx
Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)
Group: Forum Members
Posts: 8, Visits: 60
I bought the vacuum bag kit, it does not include any instructions.

What is the order to apply the cloths?

1. Peel Ply then what next ?

Reply
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
surferx - 10/14/2018 8:21:24 AM
I bought the vacuum bag kit, it does not include any instructions.

What is the order to apply the cloths?

1. Peel Ply then what next ?

Peel Ply
Perforated film
Breather cloth (at least two layers)
Vacuum bag


Edited 7 Years Ago by Steve Broad
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search