I bought the vacuum bag kit, it does not include any instructions.

What is the order to apply the cloths?

1. Peel Ply then what next ?
By Steve Broad - 10/14/2018 9:37:32 AM

surferx - 10/14/2018 8:21:24 AM
I bought the vacuum bag kit, it does not include any instructions.

What is the order to apply the cloths?

1. Peel Ply then what next ?

Peel Ply
Perforated film
Breather cloth (at least two layers)
Vacuum bag