Assuming I'm close with my estimation for pot life at 2%, I'd estimate you'll be around a 40 to 45 minute pot life at 1.5%.
If you're concerned, the easiest thing to do is just do your own gel test. Mix up 200ml at 1.5% and time how long it takes to start gelling.
|