Positioning vacuum & infusion ports on a large bonnet
Positioning vacuum & infusion ports on a large bonnet
Post Reply
Like
2
Positioning vacuum & infusion ports on a large bonnet
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
stuart321
stuart321
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 37,
Visits: 178
Hi - I have a large bonnet mould and wanted to check my thinking on positioning ports and spiral before infusing this for the first time.
It is 1.3m x 1.1m and the layup is 200gsm CF, 295gsm CF, 2mm soric (2 layers selectively used), CF reinforcing round edges and over the soric, 295gsm CF.
I was proposing to put 1 inlet centrally at the front and 2 vac ports on the 'ears' of the bonnet at the back.
I'm expecting the soric will help the infusion and it will have spiral + mesh.
Does this look a sensible approach?
Any changes you would suggest on placement?
(I know its quite a thin stack but its on a rallycar with 4 bonnet pins and we've run some really flimsy GFRP versions before so not concerned on that front).
Thanks
Stuart
Reply
Like
2
Reply
Kevin-Lee
Kevin-Lee
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 44,
Visits: 2.4K
Hi Stuart,
Maybe try this...
Yellow dot = Vac.
Purple dot = Resin Feed.
Red Line = Spiral.
Kev.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Positioning vacuum & infusion ports on a large bonnet
stuart321
-
13 Years Ago
Hi Stuart, Maybe try this... Yellow dot = Vac. Purple dot = Resin Feed. Red Line = Spiral....
Kevin-Lee
-
13 Years Ago
I suppose you've already seen the great video of Easycomposites making a Carbonfiber Bonnet?...
matthieutje65
-
13 Years Ago
Kev - thanks that looks like a good way to ensure the ears of the bonnet are properly infused....
stuart321
-
13 Years Ago
Why they make it look so easy, is because they are well prepared I guess :) When you start a...
matthieutje65
-
13 Years Ago
What kevin posted looks good, possibly with some spiral wrap for the vac side too, in the same way...
baja_patient
-
13 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search