A question about thickness


Author
Message
woodywood biker
woodywood biker
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Forum Members
Posts: 2, Visits: 19
Hi,
Before beginning any carbon fiber construction, I wish I knew what is the average thickness of 3 layers of carbon fiber 195g 2/2 twill+UD 250g +195g 2/2 twill, including the resin ?

Tx for your infos
Edited 13 Years Ago by woodywood biker
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Hi.

You can find thicknesses of the fabric you want at the EC website, in the product description.

For example, for the 195g/sqm carbon: here.

Hope it helps.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
woodywood biker
woodywood biker
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Forum Members
Posts: 2, Visits: 19
Hi,

I saw it, but the resin thichness is estimated to be zero, when 3 layers  ?

The form i have to make has not angles,  or complicated shape. It's very flat, in deed.
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Hi Woody

I usually do a few test samples that I can then examine and handle. That way you really know what you are getting.

This has saved my bacon many times. Carbon and epoxy are expensive so testing a small patch or two is time well spent.

I keep all my tests labeled so for future projects I can look at them and know in a moment what I need as far as layers.

Fred
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Thats a good way of thinking, I mostly do the same "fgayford"

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com