Hello friends,

I was studying making 3D impression moulds and sealing with epoxy resin to make carbon fiber parts in the Wet Layup + Vacuum Bagging or Vacuum infusion process. 

Has anyone done any 3D impression mould?
What better material for printing?

The composites will be cured at room temperature.

Thanks!
Replies
KOSTAS
KOSTAS
Supreme Being (301 reputation)Supreme Being (301 reputation)Supreme Being (301 reputation)Supreme Being (301 reputation)Supreme Being (301 reputation)Supreme Being (301 reputation)Supreme Being (301 reputation)Supreme Being (301 reputation)Supreme Being (301 reputation)
Group: Forum Members
Posts: 30, Visits: 244
Lester Populaire - 5/30/2018 9:24:47 PM
scottracing - 5/30/2018 11:14:56 AM
what layer height did you use on the PLA print? And did you sand it prior to the first coat of primer?

The finished part looks brilliant, is that a flax/hemp material you made the part from?

I usually print with a Layer height of 0.15 to 0.2mm and give it a light sand to get rid of small bumps where a new layer started and any things like that. Then usually two coats of heavy filler and one coat of finishing filler with wet sanding is enough to get a good finish.

The part is made from Bcomp's ampliTex 5040 fabric.


0.15 layer height !!!! How many hours did it take you  to print this bar mold ?

Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
KOSTAS - 9/12/2018 6:02:02 PM
Lester Populaire - 5/30/2018 9:24:47 PM
scottracing - 5/30/2018 11:14:56 AM
what layer height did you use on the PLA print? And did you sand it prior to the first coat of primer?

The finished part looks brilliant, is that a flax/hemp material you made the part from?

I usually print with a Layer height of 0.15 to 0.2mm and give it a light sand to get rid of small bumps where a new layer started and any things like that. Then usually two coats of heavy filler and one coat of finishing filler with wet sanding is enough to get a good finish.

The part is made from Bcomp's ampliTex 5040 fabric.


0.15 layer height !!!! How many hours did it take you  to print this bar mold ?

Many. But it's not like I was watching it... 

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Dezer - 7 Years Ago
scottracing - 7 Years Ago
Dezer - 7 Years Ago
SleepingAwake - 7 Years Ago
Dezer - 7 Years Ago
vieteejais - 5 Years Ago
scottracing - 7 Years Ago
SleepingAwake - 7 Years Ago
KostasBiz - 7 Years Ago
                     Many. But it's not like I was watching it...
SleepingAwake - 7 Years Ago
Warren (Staff) - 7 Years Ago
scottracing - 7 Years Ago
KostasBiz - 7 Years Ago
SleepingAwake - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search