Hi,
I’m using GlassCast 10 for making pen blanks. Can you please tell what is advised time to wait, after demoulding, to start turning the blank? In other words to be fully cured?
Thank you
Edited 7 Years Ago by Branco
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
We recommend a minimum of 48 hours cure time before machining.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Branco
B
Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)
Group: Forum Members
Posts: 4, Visits: 33
Thank you Warren!
Some told me that I have to wait a couple of weeks , if I want the epoxy to have a high polish. Is this the case??