By Branco - 9/9/2018 1:30:16 AM
Hi, I’m using GlassCast 10 for making pen blanks. Can you please tell what is advised time to wait, after demoulding, to start turning the blank? In other words to be fully cured? Thank you
|
By Warren (Staff) - 9/10/2018 12:21:48 PM
It is true that epoxies will continue to fully cure for that kind of time, but not that this epoxy is unpolishable. After 48 hours it is hard enough to machine and sand or polish as necessary.
|
|