GlassCast 10 full cure time.
GlassCast 10 full cure time.
Post Reply
Like
3
GlassCast 10 full cure time.
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Branco
B
Branco
posted 8 Years Ago
ANSWER
HOT
Topic Details
B
Group: Forum Members
Posts: 4,
Visits: 33
Hi,
I’m using GlassCast 10 for making pen blanks. Can you please tell what is advised time to wait, after demoulding, to start turning the blank? In other words to be fully cured?
Thank you
Edited
8 Years Ago by
Branco
Reply
Like
3
Warren (Staff)
Warren (Staff)
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
We recommend a minimum of 48 hours cure time before machining.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
4
Branco
B
Branco
posted 8 Years Ago
ANSWER
HOT
Post Details
B
Group: Forum Members
Posts: 4,
Visits: 33
Thank you Warren!
Some told me that I have to wait a couple of weeks , if I want the epoxy to have a high polish. Is this the case??
Reply
Like
3
Warren (Staff)
Warren (Staff)
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
It is true that epoxies will continue to fully cure for that kind of time, but not that this epoxy is unpolishable. After 48 hours it is hard enough to machine and sand or polish as necessary.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search