Oh, if you meant 0/90 biaxial, then its basically the same as a regular cloth of the same weight. As far as my understanding goes, every cloth with 2 fibre directions is called biaxial. Most of them are 45/-45, which are also called (at least here in Germany) bidiagonal. There are far less 0/90 biaxials, at least in the shops I use.
|