Alan here from sunny Barnsley lol
I'm making a mould for a air intake to the air box on my Ford Focus RS its an odd shape and hopefully you could help me decide how many splits on the mould I would need ?
I need to sand down the joints then cover with filler before flatting then I plan to spray it to get a really good finish 
Attachments
20180829_212928.jpg (368 views, 4.00 MB)
Replies
Barnsley-Bill
B
Supreme Being (212 reputation)Supreme Being (212 reputation)Supreme Being (212 reputation)Supreme Being (212 reputation)Supreme Being (212 reputation)Supreme Being (212 reputation)Supreme Being (212 reputation)Supreme Being (212 reputation)Supreme Being (212 reputation)
Group: Forum Members
Posts: 25, Visits: 489
This is the shape of my plug from the side 

Edited 7 Years Ago by Barnsley-Bill
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Barnsley-Bill - 8/31/2018 6:13:07 PM
This is the shape of my plug from the side 

Made from invisibelium, is it? :-)

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Barnsley-Bill - 7 Years Ago
Steve Broad - 7 Years Ago
Barnsley-Bill - 7 Years Ago
Steve Broad - 7 Years Ago
Barnsley-Bill - 7 Years Ago
Barnsley-Bill - 7 Years Ago
             Made from invisibelium, is it? :-)
Steve Broad - 7 Years Ago
Barnsley-Bill - 7 Years Ago
             Ah, the photo has now appeared :-)
Steve Broad - 7 Years Ago
Steve Broad - 7 Years Ago
Barnsley-Bill - 7 Years Ago
Steve Broad - 7 Years Ago
Barnsley-Bill - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search