By Barnsley-Bill - 8/29/2018 8:37:49 PM
Alan here from sunny Barnsley lol I'm making a mould for a air intake to the air box on my Ford Focus RS its an odd shape and hopefully you could help me decide how many splits on the mould I would need ? I need to sand down the joints then cover with filler before flatting then I plan to spray it to get a really good finish
|
By Barnsley-Bill - 9/7/2018 9:00:28 PM
Right I have my plug made and ready to start making the moulds off it but after watching the video of the split mould using the uni mold kit, I bought one then realized that its no good for the new pre peg ' would it be possible to use the EL160 is a high performance epoxy laminating resin with the glass fibre out of the uni mould kit and use the EG160 high temperature tooling gelcoat ? or if not would it be possible to make a split mould out of XPREG® XT135/S Tooling Prepreg . Thanks
ps the problem with my car not boosting was broken spring in the turbo actuator ' a not very old high performance actuator at that but at least then sent me a replacement spring that i can fit myself
|
|