I can't see this being asked on previous topics and the product pages don't specify, is the 2% MEKP ratio by weight or volume?

Warren (Staff)
Warren (Staff)
Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You can measure the catalyst by weight or volume as the density is 1g/cm3.  Often it is more convenient to have an MEKP dispenser bottle or syringe which has fine volume graduations on it than trying to weigh out the catalyst.  So in this case, you would weight out the primer and add the correct volume of MEKP from the dispenser bottle.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Matt Jones
M
Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)
Group: Forum Members
Posts: 6, Visits: 19
Thanks Warren, I've got the dispenser but the scale doesn't show the metric, do you know what it is?

Warren (Staff)
Warren (Staff)
Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The units on the bottle scale are cm3 or ml.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search