By Matt Jones - 8/28/2018 10:19:09 AM
I can't see this being asked on previous topics and the product pages don't specify, is the 2% MEKP ratio by weight or volume?
|
By Warren (Staff) - 8/28/2018 1:51:05 PM
The units on the bottle scale are cm3 or ml.
|
|