Weight came out very low. The fiberglass canopy I was using before this one weighed 165 grams. My canopy has about 10% more area, thinner walled but about same rigidity as fg canopy, 95 grams. Very impressive. 70g weight advantage on one of these helis is pretty huge. This may very well be the first resin infused heli canopy, at least that's been documented. There is one very high end brand that does vacuum bagging, but not infusion.
|