Due to moisture sensitivity you want to avoid condensation cure silicones and go for an addition cure silicone such as our AS40 Addition Cure Silicone


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
gsprk
g
Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)
Group: Forum Members
Posts: 1, Visits: 1
I have bought some Xencast P6, but from reading various posts, it may not compatible with certain types of silicone.  Can you recommend a silicone for problem free moulding / casting please.

Thanks



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search