By gsprk - 8/16/2018 7:45:13 PM
I have bought some Xencast P6, but from reading various posts, it may not compatible with certain types of silicone. Can you recommend a silicone for problem free moulding / casting please.
Thanks
|
By Warren (Staff) - 8/17/2018 8:22:45 AM
Due to moisture sensitivity you want to avoid condensation cure silicones and go for an addition cure silicone such as our AS40 Addition Cure Silicone
|
|