Which adhesive would be best for joining infused Carbon Fibre to infused Carbon Black Twaron?
There will be a constant pull on this joint.

Brian.



Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Brian,

From our range PT326 would be the one to go for; it's a rigid 2-part polyurethane structural adhesive with excellent cured mechanical properties. Polyurethanes slightly outperform epoxies for plastic-to-plastic bonding (which composite-to-composite effectively is).

Although we don't have one in our range at the moment (so this is just general advice) the other good plastic-to-plastic adhesive used in composites is methacrylate; we'll be looking at adding in a methacrylate to our range at some point. We would expect similar results to the PT326.

I hope this helps,

All the best, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Brian_s
Brian_s
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
Thank you Matt.
That is what I thought but it is best to check.

Brian.