High Temperature Pre-Preg coat


Author
Message
Abilash
A
Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)
Group: Forum Members
Posts: 4, Visits: 38
Hi! So I'm designing a part that has to go over an exhaust of a car (not too near but not too far either) so it's got constant hot air blowing over it. I've been using pre-preg carbon fiber for the part and I was wondering if I could coat it with this:

https://www.youtube.com/watch?v=-R7mm63eWv8

which I came across while browsing the internet. Was wondering what you guys would think of this if I used it as my surface gel coat for my pre-preg parts.

Thank you!
Edited 7 Years Ago by Abilash
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
X-Preg service temp is only 115C ^


The product in the video is basically an epoxy tooling gelcoat, it's intended for high temperature tooling - ie. moulds for pre-preg.

There is no point putting a high temperature surface coat on a laminate that cant handle those same temperatures. If your pre-preg parts cant handle more than 120C then having a surface coat that can handle 200C isn't going to do anything for it.
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Hanaldo - 8/13/2018 11:18:19 PM
X-Preg service temp is only 115C ^


The product in the video is basically an epoxy tooling gelcoat, it's intended for high temperature tooling - ie. moulds for pre-preg.

There is no point putting a high temperature surface coat on a laminate that cant handle those same temperatures. If your pre-preg parts cant handle more than 120C then having a surface coat that can handle 200C isn't going to do anything for it.

As the surface coat isn't a heat reflector, good point.

An option is to apply a heat reflective material, such as something from the Zircotec range. They do a self adhesive option.

https://www.zircotec.com/zircoflex/zircoflex-i/