Hi guys . Ok Im obviously new here and to bagging infusion. Im planing to make my own carbon fiber hood however this thing is huge. Almost 2 meters in width and 2 meters long. Obviously I can order as long of carbon fiber cloth as I want. But I havent been able to find a supplier that would sell a wide enough fabric as to completely cover the hood without the need to use two pieces of fabric parallel to each other in this hood. Now there might be something I dont know but my thinking is that if I lay 2 separate fabrics one next to each other for infusion in the finish product you could see the separation of the 2 and so it wouldnt look that good. 

So my question is whether there is a way to infuse a big part laying 2 separate cloth and avoid visual detection of 2 separate pieces being use and or if anyone sells a wide enough cloth to 2 meters.

Thanks 
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi,

Wow, that is a big hood. 1.5m wide is pretty much as wide as anyone weaves carbon fibre, even at 1.5m it's quite unusual but we have plenty of material up at that width. As for making a part that's wider than 1.5m without seeing a join I'm afraid you don't really have many options. I honestly don't know anyone who would supply a 2m wide roll and there really isn't any way to join the fabric without a visible join-line so you're left with these options:

1) Put an obvious 'V' herringbone join line down the middle of the hood so that instead of trying to hide the join you make a feature of it. You achieve this by rotating one of the peices of carbon by 90 degrees so that the weave comes together to make a V down the middle of the hood. You would probably need to stiffen the fibre (by spraying it with a very fine mist of epoxy) before cutting so that it is stiff enough to allow you to cut it without fraying.

2) Fade out the carbon at the edges of the panel. This is sometimes called 'executive edges' and I personally think it looks good but it's all a matter of taste. What you do is position the material in the middle of your mould so that it just comes up a little short at each side. You then infill this with some more strips of carbon before and the put the rest of your reiforcement down. You do the infusion as normal and so when you de-mould you'll just be left some ugly joins at the edges of the panel. You then spray paint black (or whatever colour your car is or you choose) from the edges, over the join and then feather out the paint as you get past the join line. It's pretty easy to spray like this, especially if it's a low-contrast scheme (i.e. black) because you can hardly see it happen. Then, once you're happy with that, you clear lacquer over the whole lot. The end result looks great and will completely hide your join lines at the edge.

I can't really think of any other ideas except other paint finishes (like a viper stripe) to hide the join but I hope this helps,

All the best, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Bchamp
Bchamp
Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)
Group: Forum Members
Posts: 2, Visits: 21
Thanks for the amazingly fast response. I re-measure and I only need 5 feet width=60 inch. I did a little digging and just found a supplier with a 60 inch wide cloth. Thanks a lot. You shall see my order on your equipment soon. Smile ....