Group: Forum Members
Posts: 2,
Visits: 14
|
Hi, I poured a glass cast 3 cover onto my penny floor yesterday. The Resin is already touch dry but there are a number of bubbles that are embedded in the resin, some below the surface some at the surface. I followed the mix by weight instructions and was expecting the bubbles to go by themselves as per the video. What can I do now to get the glass cast look that I need?
|