		| By Preece1 - 8/4/2018 6:37:04 AM 
 Hi, I poured a glass cast 3 cover onto my penny floor yesterday.  The Resin is already touch dry but there are a number of bubbles that are embedded in the resin, some below the surface some at the surface. I followed the mix by weight instructions and was expecting the bubbles to go by themselves as per the video. What can I do now to get the glass cast look that I need?
 |  
		| By Warren (Staff) - 8/7/2018 8:29:07 AM 
 120 grit sand paper dry will be fine to sand out the bubbles.  Before you pour again, just make sure the whole surface has a good key and you should be ready to go.
 
 |  |