Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Dont get me wrong, I'm all for pre-preg! I use it for most applications. I just dont think it's necessary for this job, and isn't really any more suitable than infusion is. Hes already bought the infusion kit, so for me there's no point investing more money in a different setup.
|