Dont use paint thinners, use acetone for cleaning. Or just replace each use.
24 hours is sort of the very minimum cure time for an epoxy, and that's assuming the temperature didn't drop below 25C. Ideally dont expose it to water for 72 hours unless you've done an elevated temperature cure.
|