Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
For hand layup you generally aim for a 50/50 fiber/resin fraction. So if your fabric (doesn't matter if its fibreglass or carbon or Kevlar etc) is a 360gsm, then you will need 360g of resin for every square meter of fabric. Plus a little bit of wastage factor for resin in the bottom of your cup, in your brushes, etc.
|