Hi Forum..!

I need to process by hand layup Aramid Fabrics (Kevlar) with epoxy resin. How much resin the Kevlar will need to be wetted?

Kevlar Propiertes
360 g/m2
1500 Denier
0/90°

Epoxy
Laminating epoxy, low viscosity

Thanks!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Dessert Mix - 8 Years Ago
Hanaldo - 8 Years Ago
Dessert Mix - 8 Years Ago
Hanaldo - 8 Years Ago
oekmont - 8 Years Ago
Hanaldo - 8 Years Ago
oekmont - 8 Years Ago
Steve Broad - 8 Years Ago
oekmont - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search