+x Hanaldo - 7/15/2018 6:48:12 AMSplash mould is just a quick mould that's a bit flimsier and made with cheaper materials and quickly made, figuratively 'splashing' fiberglass and resin onto the job. You can really just use regular gelcoat and general purpose polyester resin. It only needs to last one pull, so it doesn't need to be as strong as a proper mould. The important thing is to not make it so flimsy that it can warp easily and leave you with bad fitment we you make your proper mould/part.
+x Pkzipper - 7/15/2018 1:18:21 PM+x Hanaldo - 7/15/2018 6:48:12 AMSplash mould is just a quick mould that's a bit flimsier and made with cheaper materials and quickly made, figuratively 'splashing' fiberglass and resin onto the job. You can really just use regular gelcoat and general purpose polyester resin. It only needs to last one pull, so it doesn't need to be as strong as a proper mould. The important thing is to not make it so flimsy that it can warp easily and leave you with bad fitment we you make your proper mould/part.Ah yes thank you, that is what I thought.