Allergy epoxy resin


Author
Message
Miguel Angel
Miguel Angel
Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)
Group: Forum Members
Posts: 4, Visits: 65

In spanish:

Hola a todos y todas.

Quiero comentaros un caso que me ha sucedidorecientemente.

Trabajo con resinas epoxis y materiales compuestos comotejidos de carbono, carbono kevlar y otros.

Actualmente utilizo mascarilla facial solo de nariz yboca y guantes protectores además de buzo de trabajo desechable. Desde haceunos 3 días atrás me han salido unas manchas por las manos hasta el codo, en lacara igualmente las mismas manchas y además el ojo hinchado y el labio también,seguido de un pequeño picor. Pienso que ha sido los gases de catalizar lasresinas. He ido al médico y me han mandado corticoides y una crema para lasmanchas, las cuales parecen quemaduras.

Ya me ha sucedido este fenómeno varias veces a lo largodel año, con los mismos resultados.

Me han dicho que soy alérgico al catalizador de lasresinas epoxis y en du defecto a la misma resina epoxi.

Me pregunto si adquiriendo un equipo de mascarilla facialcompleta con dos juegos de filtro o en el mejor de los casos una mascarilla conaire asistido por un motor y teniendo aire en la máscara, además de colocar unextractor de aire en la habitación del taller donde trabajo me puede solucionareste imprevisto al ser alérgico a unos de los productos con los cuales trabajo.Me han comentado que cambie de resinas y que incluso pruebe con resinas ecológicascon menor  cantidad de agentes químicos habercuales son los síntomas…

 Quisiera recibir vuestras opiniones y comentariosrespecto a ello, ya que es mi medio de vida el trabajar con estos materiales.Necesito saber si probando estas mascaras completas estoy menos expuesto aestos agentes volátiles, junto a un equipo de filtración de aire del ambiente.

Espero vuestros consejos.

Os adjunto las dos clases de equipos que desearía sabersi me ayudarían.

Un saludo

Miguel A.

 

In English:
Hi all.
I mention to acase that has happened to me recently.
Working with epoxy resins and composite materials such as carbon fabric, carbon, kevlarand others.
I currently use a face mask only the nose and mouth and gloves plus disposableworking diver. Forabout three days ago I have some spots left hands to the elbowin the face equallywell the same spots and swollen eye and lipalso followed by asmall itch. I has been catalyzegases resins. Iwent to the doctor and they sentme steroids anda cream for the spots, which appear burns.
Since this phenomenon has happened to me several times throughout the year, withthe same results.
I am told that I am allergic to the catalyst of epoxyresins and du default to the same epoxyresin.
I wonder if taking on a team full face maskwith two sets of filter or in thebest case a mask with a motor-assisted air andtaking air into the mask, and put an exhaust fan in theroom of the shop where I can work around thisunforeseen to beallergic to some of the productswith which to work. I have heard that change resins and organicresins even trywith fewer chemicals have symptoms which are...

I would like to receive your opinions and comments about it, because it is my livelihood working with these materials. I need to know if I'm testing thesemasks complete lessvolatile exposed tothese agents, along with a team ofenvironmental air filtration.
I hope your advice.
I attached the two kinds of teams that would like toknow if I would help.
greetings
Miguel A.



Attachments
mascara.jpg (481 views, 46.00 KB)
MASCARAA.jpg (478 views, 174.00 KB)
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
From what I have seen most epoxies are poly amine hardeners.  There are one or two that are mercapto based.  It might be worth looking round to find a resin with a different hardener.  EC might be able to advise better than I on the properties of these resins as they might be different.  Have a look at the R numbers to see if irritation is a hazard on the different resin systems.  hope this helps?