wax sheet


Author
Message
tha_pop
tha_pop
Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)
Group: Forum Members
Posts: 17, Visits: 877
Hi, has any one used wax sheet when making molds e.g. making a cover for a part. 

after applying wax sheet to the part I applies some wax release hoping after several wax applications and polishing i will apply PVA but for some wired reason the wax reacted with the sheet and caused it to become sticky and gummy which ended up messing the smooth texture of the wax sheet Sad, has anyone had this experience and how did they overcome this issue, lastly maybe my work flow was flawed in a way and it will be great if you could point me in the right direction and share the correct steps you follow leading to a perfect mold. 
Replies
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Hi,

Here is what I did when I had to work with wax sheet:

Once the sheet was applied, I covered it with aluminium tape. Its very thin, and with meticulous placement (aka avoiding overlaps) you'll have minimal sanding work to do on your mold once you're done.

Hope it helps.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
tha_pop
tha_pop
Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)
Group: Forum Members
Posts: 17, Visits: 877
thanks, that sounds like a good option Smile