Hi,
   I've bought the carbon fibre naca vent from you which I'll be bonding to an aluminium bonnet to feed cool air to ITBs. Looking through your store the permabond 515 looked like it would fit the bill but I would appreciate some advice from someone who knows more than I do. Additionally how much would I need to bond the duct as its sold in 50ml or 400ml quantities. 
I've also been told I need to seal the aluminium before bonding carbon fibre to it otherwise it would cause corrosion. Is there a specific product for sealing it or can I just use a normal epoxy primer?

Cheers

Aaron
Reply
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
You will only need the smallest amount  - i.e. the 25 ml syringe should be enough .. that also saves you buying the "gun" for the 50 ml "cartridge"

Really you can use any good epoxy or methacrylate bonding glue it will be easily strong enough for boding in the ducts

Good luck ,and please post  pics :-D


"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Aaron Howe - 7 Years Ago
Dravis - 7 Years Ago
Aaron Howe - 7 Years Ago
Dravis - 7 Years Ago
Steve Broad - 7 Years Ago
Aaron Howe - 7 Years Ago
Steve Broad - 7 Years Ago
Aaron Howe - 7 Years Ago
Steve Broad - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search